Abstract: | Correction factors for magnetic susceptibility measurements on thin (<c. 50 mm thick > artefacts have been determined experimentally for a KT‐5 Exploranium G S. instrument using prepared blocks of Whin Sill dolerite. The cor rection factor is large (> 1.4) for samples less than 10mm thick, and reduces to 1 01 for samples of 50mm thickness. Measurements on thin samples can also be affected by the backing or substrate material on which they are measured. ‘Background’material, for example, soil or plaster, can contribute significantly to recorded measurements on artefacts, particularly for thin artefacts with low susceptibilities |