The article presents a group of Bronze Age artefacts recovered from the Drava river wetlands in continental Croatia, examining their typological and chronological markers, and assessing the technological characteristics of the material through spectrometric and use-wear analyses. We discuss the context of the finds, types of items retrieved and deposition locations, and how these fit into the patterns of European Bronze Age metal deposition practices. Compositional and metalwork use analyses indicate that most of the items were in use prior to their deposition and display solid metallurgical skill. Chronologically, typologically, compositionally, and conceptually, the items align with the depositional trends seen in the wider region and beyond.  相似文献   
2.
In the described studies with the aim of optimizing hydrated lime grout composition, the first measure was to reduce the water content of the grout using a highly efficient polycarboxylate ether-based superplasticizer, whereas the second measure was to increase the content of the inert limestone filler with an adequate grain size distribution. In this way, an attempt was made to achieve the best possible volume stability and strength properties of the hydrated lime grout, while continuing to fulfill the other necessary requirements regarding non-structural grouting works which are reported in the literature.

The results of the tests showed that a non-structural grout consisting of 1 volume part of hydrated lime CL 90-S and 3 volume parts of inert limestone filler, with 0.5% of the polycarboxylate ether based superplasticizer, fulfilled most of the established requirements, so that it is thus potentially suitable for re-attachment interventions on architectural surfaces.  相似文献   

1
设为首页 | 免责声明 | 关于勤云 | 加入收藏

Copyright©北京勤云科技发展有限公司  京ICP备09084417号